SubsTech     
SubsTech     
Command disabled: export_raw

to Halogenated solvents
to Properties of fluids

Chloroform

(submitted by the website administration)

Chlorinated solvent Chloroform
Chemical formula: CH-Cl3
Property Value in metric unit Value in US unit
Density at 68°F (20°C) 1.49*10³ kg/m³ 93.0 lb/ft³
Viscosity at 68°F (20°C) 0.57 cP 3.82*10-4 lb/ft·s
Surface tension at 68°F (20°C) 0.026 N/m 1.48*10-4 lbf/in
Vapor pressure at 68°F (20°C) 20700 Pa 3.0 psi
Boiling point 61 ºC 142 ºF
Melting Point -64 ºC -83 ºF
Autoignition temperature none ºC none ºF
Dielectric constant at 68°F (20°C) 4.79 4.79
Specific heat capacity 980 J/(kg*K) 0.234 BTU/(lb*ºF)
Latent heat of vaporization 248 kJ/kg 106.6 BTU/lb

Related internal links

chloroform.txt · Last modified: 2023/12/14 by dmitri_kopeliovich