SubsTech     
SubsTech     
Command disabled: export_raw

to Commercially pure and low alloyed titanium alloys
to Properties of titanium alloys

Commercially pure titanium, Grade 1

(submitted by the website administration)

Commercially pure titanium, Grade 1
Chemical composition: O=0.18% max., Fe=0.2% max., N=0.03% max., Ti balance
Property Value in metric unit Value in US unit
Density 4.51 *10³ kg/m³ 282 lb/ft³
Modulus of elasticity 103 GPa 15000 ksi
Thermal expansion (20 ºC) 8.6*10-6 ºCˉ¹ 4.8*10-6 in/(in* ºF)
Specific heat capacity 520 J/(kg*K) 0.124 BTU/(lb*ºF)
Thermal conductivity 20.8 W/(m*K) 144 BTU*in/(hr*ft²*ºF)
Electric resistivity 54*10-8 Ohm*m 54*10-6 Ohm*cm
Tensile strength 331 MPa 48000 psi
Yield strength 241 MPa 35000 psi
Elongation 30 % 30 %
Hardness 70 HRB 70 HRB
Melting temperature 1670 ºC 3040 ºF
Beta Transus temperature 890 ºC 1630 ºF