Nickel occurs in ores of two general types:

  • nickel-iron sulfides,
  • hydrous nickel silicate (laterite).

Both of them typically contain 1-3% of nickel.

Extraction of nickel from sulfide ores

Extraction of nickel from sulfide oresis carried out by the following process:

  • Crushing and grinding the ore in order to free the gangue from the nickel sulfide mineral.
  • Concentrating – separation of the nickel sulfide mineral from the gangue.

This operation is conducted in a flotation chamber where the ground ore mixed with water is treated by air bubbles which move upward and cause flotation of the mineral particles to the top of the chamber.

  • Smelting or roasting with partial converting sulfides to oxide form.
  • Matte smelting.

At this stage the concentrate is smelted in the Bessemer converter to produce a mixture of nickel, copper and other metals called matte.

The gangue is absorbed by the slag and removed.

  • Electrolytic or chemical refining of nickel.

Extraction of nickel from the laterite ores

Extraction of nickel from the laterite ores is carried out by either pyrometallurgical or hydrometallurgical process:

  • Hydrometallurgical process involves ammoniacal or sulfuric acid leaching followed by nickel precipitatation.
  • In the pyrometallurgical process the ore is dried and calcined in a rotary kiln and then smelted in an electric furnace with addition of carbon. The resulted nickel-iron matte may be either further refined or used as desired product (in this case sulfur in form of gypsum or elemental sulfur is added to the kiln).

to top


Related internal links

extractive_metallurgy_of_nickel.txt · Last modified: 2023/12/13 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License