Chemical composition: carbon (C)
Property Value in metric unit Value in US unit
Density 1.7*10³ kg/m³ 106 lb/ft³
Porosity 11 % 11 %
Flexural strength 55 MPa 7980 psi
Compressive strength 155 MPa 22475 psi
Hardness 85 scleroscope 85 scleroscope
Thermal expansion (20 ºC) 3*10-6 ºCˉ¹ 1.7*10-6 in/(in* ºF)
Thermal conductivity 120 W/(m*K) 832 BTU*in/(hr*ft²*ºF)
Max. service temperature 399 °C 750 ºF


Applications: bearings, bushings.