| Silicate ceramic Cordierite C410 | ||||
| Chemical composition: 3Al2O3*2SiO2, Al2O3, SiO2 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 2.1 *10³ | kg/m³ | 131.1 | lb/ft³ | 
|---|---|---|---|---|
| Flexural strength | 60 | MPa | 8700 | psi | 
| Thermal expansion (20 ºC) | 2.0*10-6 | ºCˉ¹ | 1.1*10-6 | in/(in* ºF) | 
| Thermal conductivity | 2.0 | W/(m*K) | 13.9 | BTU*in/(hr*ft²*ºF) | 
| Dielectric constant | 6 | - | 6 | - | 
 