Strong Cation Exchange Resin in hydrogen form | ||||
Uniform Particle Size, High Capacity Strong Acid Cation Exchange Resin | ||||
Property | Value in metric unit | Value in US unit | ||
Matrix | Styrene-DVB, gel | |||
---|---|---|---|---|
Functional group | Sulfonic acid | |||
Exchange capacity | 2 | eq/l | 43.7 | kgr of CaCO3/ft³ |
Water content | 45% | |||
Total swelling (Na+ → H+) | 8% | |||
Mean particle size | 0.59 | mm | 23.2 | μinch |
Particle density | 1.28 | kg/l | 79.9 | lb/ft³ |
Shipping weight | 0.82 | kg/l | 51 | lb/ft³ |
Maximum work temperature | 120 | °C | 250 | °F |
PH range | 0-14 | |||
Min. bed depth | 800 | mm | 2.6 | ft |
Service flow rate | 5-60 | m/h | 2-24 | gpm/ft2 |
Co-current regeneration rinse | 1-10 | m/h | 0.4-4 | gpm/ft2 |
Counter-current regeneration rinse | 5-20 | m/h | 2-8 | gpm/ft2 |
Total rinse requirement | 2-5 bed volumes | |||
Regenerant | H2SO4 (1-8%) or HCl (4-8%) |