Aluminum cutting fluid | ||||
Mineral oil and natural esters based fluid | ||||
Property | Value in metric unit | Value in US unit | ||
Density at 60°F (15.6°C) | 0.905 *10³ | kg/m³ | 56.5 | lb/ft³ |
---|---|---|---|---|
Kinematic viscosity at 104°F (40°C) | 22.3 | cSt | 22.3 | cSt |
Flash point | 182 | ºC | 360 | ºF |
Pour Point | -20 | ºC | -4 | ºF |
Applications: machining of non-ferrous metals: aluminum, brass, bronze, copper, and magnesium.