to Halogenated solvents
to Properties of fluids
(submitted by the website administration)
| Chlorinated solvent Carbon tetrachloride | ||||
| Chemical formula: CCl4 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 68°F (20°C) | 1.58*10³ | kg/m³ | 98.6 | lb/ft³ |
|---|---|---|---|---|
| Viscosity at 68°F (20°C) | 0.97 | cP | 6.52*10-4 | lb/ft·s |
| Surface tension at 68°F (20°C) | 0.027 | N/m | 1.54*10-4 | lbf/in |
| Vapor pressure at 68°F (20°C) | 11940 | Pa | 1.73 | psi |
| Boiling point | 77 | ºC | 171 | ºF |
| Melting Point | -23 | ºC | -9.4 | ºF |
| Autoignition temperature | none | ºC | none | ºF |
| Dielectric constant at 68°F (20°C) | 2.24 | 2.24 | ||
| Specific heat capacity | 840 | J/(kg*K) | 0.201 | BTU/(lb*ºF) |
| Latent heat of vaporization | 190 | kJ/kg | 81.7 | BTU/lb |