| Chlorinated solvent Chloroform | ||||
| Chemical formula: CH-Cl3 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 68°F (20°C) | 1.49*10³ | kg/m³ | 93.0 | lb/ft³ |
|---|---|---|---|---|
| Viscosity at 68°F (20°C) | 0.57 | cP | 3.82*10-4 | lb/ft·s |
| Surface tension at 68°F (20°C) | 0.026 | N/m | 1.48*10-4 | lbf/in |
| Vapor pressure at 68°F (20°C) | 20700 | Pa | 3.0 | psi |
| Boiling point | 61 | ºC | 142 | ºF |
| Melting Point | -64 | ºC | -83 | ºF |
| Autoignition temperature | none | ºC | none | ºF |
| Dielectric constant at 68°F (20°C) | 4.79 | 4.79 | ||
| Specific heat capacity | 980 | J/(kg*K) | 0.234 | BTU/(lb*ºF) |
| Latent heat of vaporization | 248 | kJ/kg | 106.6 | BTU/lb |