to Elastomers
to Properties of polymers
(submitted by the website administration)
| Elastomer | ||||
| Polyisoprene (natural rubber) | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 0.93 *10³ | kg/m³ | 58.1 | lb/ft³ |
|---|---|---|---|---|
| Tensile strength | 20 | MPa | 2900 | psi |
| Elongation | 800 | % | 800 | % |
| Glass transition temperature | -70 | ºC | -94 | ºF |
| Maximum work temperature | 80 | ºC | 176 | ºF |
| Electric resistivity | 107-109 | Ohm*m | 109-1011 | Ohm*cm |
| Dielectric constant | 2.7 | - | 2.7 | - |
Applications: automobile tires, gaskets, hoses.