| Fast curing cyanoacrylate adhesive | ||||
| Single component moisture activated curing cyanoacrylate adhesives | ||||
| Property | Value in metric unit | Value in US unit | ||
| Viscosity at 77°F (25°C) | 2 | cP | 4.18*10-5 | lbf*sec/ft² |
|---|---|---|---|---|
| Fixture time, steel, 77°F (25°C) | 3 | min | 3 | min |
| Maximum gap | 0.051 | mm | 0.002 | in |
| Shear strength, steel, 77°F (25°C) | 20 | MPa | 2900 | psi |
| Min. service temperature | -54 | ºC | -65 | ºF |
| Max. service temperature | 180 | ºC | 82 | ºF |