to Quenching and heat transfer oils
to Properties of fluids
(submitted by the website administration)
| Heat tranfer oil ISO 100 | ||||
| Mineral based oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.890 *10³ | kg/m³ | 55.6 | lb/ft³ |
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 90.2 | cSt | 90.2 | cSt |
| Kinematic viscosity at 212°F (100°C) | 10.6 | cSt | 10.6 | cSt |
| Viscosity index | 100 | 100 | ||
| Flash point | 267 | ºC | 512 | ºF |
| Pour Point | -9 | ºC | 14 | ºF |
| Color | 0.5 | 0.5 | ||
| Thermal conductivity at 104°F (40°C) | 0.0106 | W/m*K | 0.073 | BTU*in/(hr*ft²*ºF) |
| Specific heat capacity at 104°F (40°C) | 1950 | J/(kg*K) | 0.47 | BTU/(lb*ºF) |
Applications: heat transfer oil in closed circulation systems operating at temperatures up to 320ºC (620ºF), quenching oil for heat treating steels.