to Quenching and heat transfer oils
to Properties of fluids
(submitted by the website administration)
| Heat tranfer oil ISO 32 | ||||
| Mineral based paraffinic oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.890 *10³ | kg/m³ | 55.6 | lb/ft³ |
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 33.4 | cSt | 33.4 | cSt |
| Flash point | 216 | ºC | 420 | ºF |
| Pour Point | -15 | ºC | 5 | ºF |
Applications: heat transfer oil in open circulation systems and in closed circulation systems operating at temperatures up to 288ºC (550ºF), quenching oil.