| High thermal conductivity isostatically pressed graphite | ||||
| Chemical composition: carbon (C) | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.90*10³ | kg/m³ | 119 | lb/ft³ |
|---|---|---|---|---|
| Modulus of elasticity | 11.8 | GPa | 1710 | ksi |
| Flexural strength | 53.9 | MPa | 7820 | psi |
| Compressive strength | 103 | MPa | 14940 | psi |
| Tensile strength | 29.4 | MPa | 4260 | psi |
| Hardness (Shore) | 60 | HS | 60 | HS |
| Thermal expansion (20 ºC) | 4.8*10-6 | ºCˉ¹ | 2.7*10-6 | in/(in* ºF) |
| Thermal conductivity | 139 | W/(m*K) | 963 | BTU*in/(hr*ft²*ºF) |
| Electric resistivity | 9.5*10-6 | Ohm*m | 9.5*10-4 | Ohm*cm |
Applications: Non-ferrous metals metallurgy and semiconductors fabrication.