Metal Matrix Composite Al-2%Cu-60% Al2O3 fiber | ||||
Composition: Aluminum alloy (2%Cu)+ 60 vol.% Al2O3 continuous fibers | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 3.4 *10³ | kg/m³ | 212 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity (long.) | 240 | GPa | 34800 | ksi |
Modulus of elasticity (trans.) | 160 | GPa | 23200 | ksi |
Tensile strength (longitude.) | 1500 | MPa | 217550 | psi |
Compressive strength (long.) | 3400 | MPa | 493100 | psi |