| Nitride Bonded Silicon Carbide (NSC) | ||||
| Chemical composition: SiC | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 2.82*10³ | kg/m³ | 176 | lb/ft³ |
|---|---|---|---|---|
| Modulus of elasticity | 195 | GPa | 28300 | ksi |
| Flexural strength | 200 | MPa | 29000 | psi |
| Thermal expansion (20 ºC) | 4.2*10-6 | ºCˉ¹ | 2.3*10-6 | in/(in* ºF) |
| Thermal conductivity | 14.5 | W/(m*K) | 101 | BTU*in/(hr*ft²*ºF) |
| Max. working temperature | 1450 | ºC | 2640 | ºF |