to Halogenated solvents
to Properties of fluids
(submitted by the website administration)
| Chlorinated solvent Perchlorethylene | ||||
| Chemical formula: Cl2C=CCl2 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 68°F (20°C) | 1.62*10³ | kg/m³ | 101.3 | lb/ft³ |
|---|---|---|---|---|
| Viscosity at 68°F (20°C) | 0.80 | cP | 5.37*10-4 | lb/ft·s |
| Surface tension at 68°F (20°C) | 0.032 | N/m | 1.83*10-4 | lbf/in |
| Vapor pressure at 68°F (20°C) | 1900 | Pa | 0.276 | psi |
| Boiling point | 121 | ºC | 250 | ºF |
| Melting Point | -22 | ºC | -7.6 | ºF |
| Autoignition temperature | none | ºC | none | ºF |
| Dielectric constant at 77°F (25°C) | 2.36 | 2.36 | ||
| Specific heat capacity | 900 | J/(kg*K) | 0.215 | BTU/(lb*ºF) |
| Latent heat of vaporization | 209 | kJ/kg | 89.9 | BTU/lb |