| Silicate ceramic Alumina Porcelain C110 | ||||
| Chemical composition: SiO2, Al2O3 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 2.45 *10³ | kg/m³ | 153.0 | lb/ft³ |
|---|---|---|---|---|
| Flexural strength | 40 | MPa | 5800 | psi |
| Compressive strength | 450 | MPa | 65300 | psi |
| Thermal expansion (20 ºC) | 5.2*10-6 | ºCˉ¹ | 2.9*10-6 | in/(in* ºF) |
| Thermal conductivity | 1.9 | W/(m*K) | 13.2 | BTU*in/(hr*ft²*ºF) |
| Dielectric constant | 6 | - | 6 | - |