Uniform Particle Size, High Capacity Strong Acid Cation Exchange Resin
Property Value in metric unit Value in US unit
Matrix Styrene-DVB, gel
Functional group Sulfonic acid
Exchange capacity 1.8 eq/l 39.3 kgr of CaCO3/ft³
Water content 53%
Total swelling (Na+ → H+) 8%
Mean particle size 0.60 mm 23.6 μinch
Particle density 1.20 kg/l 78.6 lb/ft³
Shipping weight 0.80 kg/l 50 lb/ft³
Maximum work temperature 120 °C 250 °F
PH range 0-14
Min. bed depth 800 mm 2.6 ft
Service flow rate 5-60 m/h 2-24 gpm/ft2
Co-current regeneration rinse 1-10 m/h 0.4-4 gpm/ft2
Counter-current regeneration rinse 5-20 m/h 2-8 gpm/ft2
Total rinse requirement 2-5 bed volumes
Regenerant NaCl (8-12%)