Synthetic cutting fluid concentrate | ||||
Synthetic fluid | ||||
Property | Value in metric unit | Value in US unit | ||
Density at 60°F (15.6°C) | 1.085 *10³ | kg/m³ | 67.7 | lb/ft³ |
---|---|---|---|---|
PH | 9.8 | 9.8 | ||
Acid value | 44 | meqKOH/g | 44 | meqKOH/g |
Used in water diluted condition at concentrations 4-7%. Applications: grinding,sawing, drilling, tapping, milling, turning.