to Elastomers
to Properties of polymers
(submitted by the website administration)
| Thermoplastic Elastomer | ||||
| Styrene-Butadiene | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 0.99*10³ | kg/m³ | 61.8 | lb/ft³ |
|---|---|---|---|---|
| Tensile strength | 14 | MPa | 2030 | psi |
| Elongation | 700 | % | 700 | % |
| Maximum work temperature | 80 | ºC | 176 | ºF |
Applications: food packaging, conveyor belts, disposable medical products, wire and cable isolation, tires, shoe soles