| Thermoset | ||||
| Alkyds (AMC), mineral filled | ||||
| Property | Value in metric unit | Value in US unit | ||
| Modulus of elasticity | 12 | GPa | 1800 | ksi |
|---|---|---|---|---|
| Tensile strength | 45 | MPa | 6500 | psi |
| Flexural yield strength | 90 | MPa | 13000 | psi |
| Compressive strength | 170 | MPa | 25000 | psi |
| Thermal expansion (20 ºC) | 36*10-6 | ºCˉ¹ | 20*10-6 | in/(in* ºF) |
| Maximum work temperature | 190 | ºC | 375 | ºF |
Applications: circuit breakers, switch gears, colored parts.