| Aromatic solvent Toluene | ||||
| Chemical formula: C6H5CH3 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 68°F (20°C) | 0.87 *10³ | kg/m³ | 54.3 | lb/ft³ |
|---|---|---|---|---|
| Viscosity at 68°F (20°C) | 0.59 | cP | 3.96*10-4 | lb/ft·s |
| Surface tension at 68°F (20°C) | 0.029 | N/m | 1.66*10-4 | lbf/in |
| Vapor pressure at 68°F (20°C) | 29 | torr | 29 | torr |
| Boiling point | 111 | ºC | 232 | ºF |
| Melting Point | -95 | ºC | -139 | ºF |
| Flash Point | 4 | ºC | 40 | ºF |
| Dielectric constant at 77°F (25°C) | 2.38 | 1.88 | ||
| Dipole moment at 68°F (20°C) | 0.31 | Debye | 0.31 | Debye |
| Color | Colorless | Colorless | ||