to Halogenated solvents
to Properties of fluids
(submitted by the website administration)
| Chlorinated solvent Trichlorethylene | ||||
| Chemical formula: ClCH-CCl2 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 68°F (20°C) | 1.46*10³ | kg/m³ | 91.4 | lb/ft³ |
|---|---|---|---|---|
| Viscosity at 68°F (20°C) | 0.58 | cP | 3.89*10-4 | lb/ft·s |
| Surface tension at 68°F (20°C) | 0.032 | N/m | 1.82*10-4 | lbf/in |
| Vapor pressure at 68°F (20°C) | 7900 | Pa | 1.15 | psi |
| Boiling point | 87 | ºC | 189 | ºF |
| Melting Point | -86 | ºC | -123 | ºF |
| Autoignition temperature | 410 | ºC | 770 | ºF |
| Dielectric constant at 68°F (20°C) | 3.27 | 3.27 | ||
| Specific heat capacity | 930 | J/(kg*K) | 0.222 | BTU/(lb*ºF) |
| Latent heat of vaporization | 241 | kJ/kg | 103.6 | BTU/lb |