to Classification of adhesives
to Properties of polymers
(submitted by the website administration)
| Two component fast curing epoxy adhesive | ||||
| Two component, clear, non-yellowing fast curing epoxy adhesive | ||||
| Property | Value in metric unit | Value in US unit | ||
| Viscosity (mixed) at 77°F (25°C) | 12000 | cP | 0.251 | lbf*sec/ft² |
|---|---|---|---|---|
| Working strength time | 5 | min | 5 | min |
| Full cure time | 24 | hrs | 24 | hrs |
| Maximum gap | 2 | mm | 0.08 | in |
| Shear strength, steel-to-steel 77°F (25°C) | 13 | MPa | 1885 | psi |
| Peel strength, steel-to-steel 77°F (25°C) | 45 | N/(25mm width) | 10 | PIW (lbf/inch width) |
| Min. service temperature | -40 | ºC | -40 | ºF |
| Max. service temperature | 80 | ºC | 175 | ºF |