| Commercially pure nickel 301 | ||||
| Chemical composition: Al=4.4%, Ti=0.6%, Ni balance | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 8.26 *10³ | kg/m³ | 516 | lb/ft³ |
|---|---|---|---|---|
| Modulus of elasticity | 207 | GPa | 30000 | ksi |
| Thermal expansion (20 ºC) | 12.9*10-6 | ºCˉ¹ | 7.2*10-6 | in/(in* ºF) |
| Specific heat capacity | 435 | J/(kg*K) | 0.104 | BTU/(lb*ºF) |
| Thermal conductivity | 40.4 | W/(m*K) | 280 | BTU*in/(hr*ft²*ºF) |
| Electric resistivity | 42.4*10-8 | Ohm*m | 42.4*10-6 | Ohm*cm |
| Tensile strength (annealed) | 462 | MPa | 67000 | psi |
| Yield strength (annealed) | 148 | MPa | 21500 | psi |
| Elongation (annealed) | 45 | % | 45 | % |
| Solution temperature | 925 | ºC | 1700 | ºF |
| Aging temperature | 588 | ºC | 1090 | ºF |
| Aging time | 16 | Hrs. | 16 | Hrs. |