Single component moisture activated curing cyanoacrylate adhesives
Property Value in metric unit Value in US unit
Viscosity at 77°F (25°C) 23000 cP 0.480 lbf*sec/ft²
Fixture time, steel, 77°F (25°C) 15 min 15 min
Maximum gap 0.508 mm 0.02 in
Shear strength, steel, 77°F (25°C) 21 MPa 3100 psi
Min. service temperature -54 ºC -65 ºF
Max. service temperature 180 ºC 82 ºF