| Polyvinyl acetate adhesive | ||||
| High viscosity homopolymer aqueous emulsion of vinyl acetate stabilised with polyvinyl alcohol | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.10 *10³ | kg/m³ | 68.7 | lb/ft³ |
|---|---|---|---|---|
| Viscosity at 77°F (25°C) | 15000 | cP | 0.313 | lbf*sec/ft² |
| PH | 3 | 3 | ||
| Particle size | 0.5-3 | mkm | 2-12*10-5 | in |
| Solids | 50 | % | 50 | % |
| Min. bonding temperature | 2 | ºC | 36 | ºF |
| Service temperature range | 5-30 | ºC | 41-86 | ºF |