Hi-Nicalon type S | ||||
Composition: Silicon carbon (SiC) matrix + SiC long (cont.) fibers (12 mkm diameter) | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 3.04 *10³ | kg/m³ | 190 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 420 | GPa | 60900 | ksi |
Thermal heat capacity | 630 | J/(kg*K) | 0.15 | BTU/(lb*ºF) |
Thermal conductivity | 18 | W/(m*K) | 125 | BTU*in/(hr*ft²*ºF) |