Uniform Particle Size, High Capacity Strong Acid Cation Exchange Resin
Property Value in metric unit Value in US unit
Matrix Styrene-DVB, gel
Functional group Sulfonic acid
Exchange capacity 2 eq/l 43.7 kgr of CaCO3/ft³
Water content 45%
Total swelling (Na+ → H+) 8%
Mean particle size 0.59 mm 23.2 μinch
Particle density 1.28 kg/l 79.9 lb/ft³
Shipping weight 0.82 kg/l 51 lb/ft³
Maximum work temperature 120 °C 250 °F
PH range 0-14
Min. bed depth 800 mm 2.6 ft
Service flow rate 5-60 m/h 2-24 gpm/ft2
Co-current regeneration rinse 1-10 m/h 0.4-4 gpm/ft2
Counter-current regeneration rinse 5-20 m/h 2-8 gpm/ft2
Total rinse requirement 2-5 bed volumes
Regenerant H2SO4 (1-8%) or HCl (4-8%)