Way lubricant ISO 32

(submitted by the website administration)

Way lubricant ISO 32
Mineral based oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.872 *10³ kg/m³ 54.5 lb/ft³
Kinematic viscosity at 104°F (40°C) 33.3 cSt 33.3 cSt
Kinematic viscosity at 212°F (100°C)/) 5.6 cSt 5.6 cSt
Viscosity index 104 104
Flash point 236 ºC 456 ºF
Pour Point -12 ºC -10 ºF
Total acid No. 1.29 1.29
Color 1.5 1.5