| Gun rust protection oil ISO 11 | ||||
| Mineral based oil with corrosion inhibitor | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.892 *10³ | kg/m³ | 55.7 | lb/ft³ |
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 11.0 | cSt | 11.0 | cSt |
| Kinematic viscosity at 212°F (100°C) | 3.0 | cSt | 3.0 | cSt |
| Flash Point | 160 | ºC | 320 | ºF |
| Pour Point | -57 | ºC | -71 | ºF |
| Viscosity index | 133 | 133 | ||
| Coverage | 125 | m²/l | 5100 | ft²/gal |
Applications: lubrication, corrosion protection and indoor storage of of small parts and small arms.