| Industrial gear oil ISO 150 | ||||
| Mineral based gear oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.884 *10³ | kg/m³ | 55.2 | lb/ft³ |
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 149.7 | cSt | 149.7 | cSt |
| Kinematic viscosity at 212°F (100°C) | 14.8 | cSt | 14.8 | cSt |
| Viscosity index | 98 | 98 | ||
| Timken OK load | 27.5 | kg | 60.6 | lb. |
| Flash point | 256 | ºC | 493 | ºF |
| Pour Point | -24 | ºC | -11 | ºF |
| AGMA No. | 4EP | 4EP | ||
| Color | 3.5 | 3.5 | ||