| Engine oil SAE 5W-20 | ||||
| Mineral based multigrade gasoline engine oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.850 *10³ | kg/m³ | 53.1 | lb/ft³ |
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C)/100°F (38°C) | 45.2 | cSt | 228 | SSU |
| Kinematic viscosity at 212°F (100°C)/210°F (99°C) | 8.4 | cSt | 56 | SSU |
| Viscosity index | 163 | 163 | ||
| CCS viscosity at -22°F (-30°C) | 4000 | cP | 4000 | cP |
| Flash point | 214 | ºC | 420 | ºF |
| Pour Point | -40 | ºC | -40 | ºF |
| Sulfated ash | 0.83 | % | 0.83 | % |
| Neutralization No. (TBN-E) | 7.5 | 7.5 | ||
| Color | 2 | 2 | ||